Technical Data Sheet

Technical Data Sheet

Complete before-curing and after-curing data for our Inorganic Silicon Oxide cooling exchanger chemical. Mix 5:1, apply a 1–2 mm layer, and achieve full cure in 40 minutes at room temperature.

Technical Data Sheet

Technical Data Sheet

Before Curing

ParameterUnitValue
Basic RMMetal Oxide, Isocynate, Silcazel, additives
ColourOff White
Densityg/cm³2.1 g/cm³
ViscositymPa·s201,000–227,000 mPa·s (cP)

After Curing

ParameterUnitValue
ColourOff White
Densityg/cm³2.1 g/cm³
ViscositymPa·s201,000–227,000 mPa·s
HardnessShore D75–80 (7,000–12,000 PSI)
Tensile StrengthMPa34–48 MPa (5,000–7,000 PSI)
Elongation at Break%1–5 %
Shear Strength (Al)MPa20–25 MPa
Volume ResistivityΩ·cm10⁵ Ω·cm
Surface ResistivityΩ·cmLess than 10⁵ Ω·cm
Thermal ConductivityW/m·K50–300 W/m·K
Working Temperature°C25 °C
Flame RetardancyUL 94Non-flammable
RoHS CompliantYes
Halogen CompliantHalogen-Free
REACH CompliantYes
Shelf LifeMonths24 months

Tested in defreezer cooling test and furnace hardness test. Salt-spray verified by Indiana Test, Calibration & Certification Services (TC-5982).

Precautions

Store in a cool, dry place with the container tightly closed to avoid moisture and water contact. See the Applications page for the four-step application guide.